Support
Machine type
Brand
Vastex EconoRed II, III and VI Infrared Conveyor Dryers

Vastex EconoRed cure settings: temperature, heater height, belt speed, exhaust, start-up and shutdown

✓ Reviewed by Jason KimUpdated 2 min readFits: EconoRed II · EconoRed III · EconoRed VI
Short answer

Start the belt before the heat, and never stop it while the heaters are above 300°F. For plastisol Vastex suggests starting at an 800°F set point, heaters 3 in above the garment, about 30 seconds in the chamber and the exhaust at 25%. The controller reads the heater, not the ink, so check the ink itself reaches 310 to 320°F. At shutdown, turn the heat off and keep the belt running until the dryer drops to 300°F.

Three things control the cure on an EconoRed: the temperature set point, the heater height and the belt speed. Dryers built from June 2024 also have a variable exhaust. Change one at a time and test.

Start-up

  1. Main power

    Turn the main power switch on the side of the control box to ON. The red power light comes on.

  2. Clear the belt

    Remove anything from the conveyor and belt.

  3. Power switch

    Turn on the power switch. The belt speed control and heat switch get power and the exhaust fan starts.

  4. Belt

    Turn on the conveyor and set your speed.

  5. Heat

    Turn on the heat switch. Hold the up arrow on the controller to raise the set value; it climbs faster the longer you hold it. Allow about 15 minutes to heat up.

  6. Exhaust

    Unlock the knob near the stack and slide it to your flow percentage.

The belt must be moving whenever the heaters are above 300°F (149°C).

Starting settings

Setting Plastisol Water-based or discharge
Ink must reach 310 to 320°F Full cure after the water evaporates
Set point 800°F Lower as time goes up
Heater height About 3 in (2 to 3 in range) 2 to 3 in
Time in chamber 20 to 30 seconds 50 to 90 seconds
Exhaust 25% Enough to clear steam and fumes

Vastex stresses these are starting points. Garment moisture and color, ink color and thickness, and room conditions all change the result.

Adjusting

  • Heater height: turn the crank on top clockwise to raise the heaters, counterclockwise to lower them.
  • Belt speed: turn the knob clockwise to speed up. The volt meter shows the volts going to the motor. Your dryer has a label on the control box that converts volts to time in the chamber; always confirm with a stopwatch.
  • Exhaust: use just enough to stop smoke escaping at the ends. Too much cools the area under the first and last heaters, and above 50% film and paper can lift.
  • Idle time: if nothing runs for over 10 minutes, drop the set point to 500°F.

Check the cure

The sensor reads the heater face, so measure the ink. A contact thermocouple (donut probe) is the most accurate. A heat gun reads cooler than the real ink temperature; if you use one, aim at the ink while it's still under the last heater, near the outside of the print. Wash test new combinations.

Shutdown

  1. Heat off

    Turn off the heat switch and let the heaters fall to 300°F or lower with the belt still running.

  2. Belt off (optional)

    Once at 300°F, turn the belt speed down to off, or leave it set for the next shift.

  3. Power switch

    Turn the power switch off. Only the power light should still be on.

  4. Main power

    Turn the main power switch OFF at the end of every shift. No lights should be on.

If prints come out under cured even at slow speeds, text us your settings and a photo at (562) 609-4996.

Watch Vastex's video: EconoRed settings to cure plastisol

Embedded from the manufacturer's official channel.

Common questions

Why is my set point so much higher than the cure temperature?

The sensor sits right under the heater, so it reads far hotter than the garment. Vastex has you set it several hundred degrees above the ink cure temperature.

How long does it take to heat up?

About 15 minutes to reach 700 to 800°F.

What's the best way to check cure temperature?

A contact thermocouple such as a donut probe is most accurate. A laser gun reads low; if you use one, aim at the ink while it's still under the last heater, toward the outside of the print.

Film or paper blows around in the chamber.

Turn the exhaust down. Vastex says light items go airborne above about 50%.

Nothing is going through for a while. Should I turn it off?

If it's idle more than 10 minutes, Vastex suggests dropping the set point to 500°F. It takes about 10 minutes to come back up.

Sources
Did this fix it?